  The location of casting peeling is often on larger flat surfaces, curved surfaces, or near sharp corners. Obvious peeling can only be clearly observed after shot blasting. So what is the reason for peeling? Firstly, due to uneven filling or slow flow caused by splashing, the metal liquid entering the mold cavity first fails to fully fuse with the subsequent metal liquid, resulting in weak bonding of the substrate and causing surface peeling. 2、 High impact pressure or mold deformation during die casting. 3、 The mold temperature is not suitable, or the runner design is unreasonable. 4、 The impact of release agents, different release agents have different focuses, and some release agents may have an impact on peeling. 5、 Peeling is also related to shot blasting, which can be improved by changing the material of shot blasting or reducing the time of shot blasting.

indirect squeeze casting

Read recommendations:

precision metal stamping parts

formlabs injection molding

aluminum profile

aluminium extrusion profile 40 series.Will baking paint on aluminum alloy die castings peel off

Do you know why the surface of aluminum alloy castings undergoes oxidation and blackening